Material | Alloy type | Size | D50 [µm] |
TD [g/cm3] |
(H/T) | O [ppm] |
Hc [Oe] |
Mm [emu/g] |
True Density [g/cm3] |
---|---|---|---|---|---|---|---|---|---|
Fe-Si | PIS35M | PF-10F | 6 | 3.9 | - | 6600 | 10.2 | 205 | 7.6 |
PF-20F | 11 | 4.3 | - | 4300 | 10.3 | 205 | |||
-75µm | 40 | - | - | 2800 | 8.0 | 205 | |||
Fe-Si-Cr | EA-SMP-10 | PF-20F | 11 | 4.3 | - | 2500 | 14.2 | 190 | 7.6 |
800° | 1600 | 10.3 | 190 | ||||||
Fe-Si-Al | SENDUST | PF-20F | 10 | 4.0 | - | 3500 | 4.0 | 110 | 7.1 |
800℃ | 3600 | 2.0 | 110 | ||||||
Permalloy | Fe-50%Ni | PF-20F | 10 | 4.5 | - | 1800 | 12.8 | 155 | 8.2 |
800℃ | 1100 | 3.1 | 155 | ||||||
Fe Amorphous |
AW2-08 | PF-20F | 11 | 4.4 | - | 1600 | 1.6 | 150 | 7.0 |
500° | 1600 | 0.7 | 150 | ||||||
KUAMET®6B2 (SWAP®) |
-150µm | 50 | - | - | 300 | 1.2 | 150 | ||
500° | - | 0.5 | 150 |
* KUAMET® and SWAP® are our trademarks.
![]() a)Amorphous Cores |
![]() b)SMD Cores |
Apps Power inductor Choke Coils SMD Coils Reactors Printer Yokes Shield Materials |
Fe-Si
Fe-Si-Cr
Fe-Si-Al
Fe-Cr
Fe-Ni
Fe-Co
Fe
Base Amorphous
Co
Base Amorphous
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |